FINALLY, A KYNAR® GRADE FOR SEALS, O-RINGS, AND DIAPHRAGMS
Kynar UltraFlex™ is an elastomeric material based on Arkema's proven PVDF (polyvinylidene fluoride) resin. This unique fluoropolymer exhibits exceptional resistance to chemicals, ozone, ultraviolet light, radiation and moisture. Molding is very similar to many fluoroelastomers without the use of curing agents and molding time is significantly reduced. Post-curing of molded parts improves mechanical properties and chemical resistance.
PVDF Elastomers
KYNAR ULTRAFLEX™ Elastomer is a clear elastomeric fluoropolymer that resists chemicals, ozone. UV rays, radiation and moisture.
Kynar UltraFlex™ is an elastomeric material based on Arkema's proven PVDF (polyvinylidene fluoride) resin. This unique fluoropolymer exhibits exceptional resistance to chemicals, ozone, ultraviolet light, radiation and moisture. Molding is very similar to many fluoroelastomers without the use of curing agents and molding time is significantly reduced. Post-curing of molded parts improves mechanical properties and chemical resistance.
PVDF Elastomers
- Clear Elastomeric Fluoropolymer
- Not Affected by UV or Radiation
- Weatherable
- Water Repellent
- Broad Chemical Resistance
- No Curing or Cross-Linking Agents
- No Shelf Life for Feed Stock
KYNAR ULTRAFLEX™ Elastomer is a clear elastomeric fluoropolymer that resists chemicals, ozone. UV rays, radiation and moisture.
Unit of Measure
Specifications
Durometer Hardness |
N/A 55 Shore A |
Firmness |
N/A 15 Firmness Rating Scale |
Tensile Strength |
N/A 825 lb/in² |
Elongation |
N/A 730 % |
Specific Gravity |
N/A 1.78 g/cc |
Density |
N/A 111 lb/ft³ |
Minimum Temperature |
N/A -15 ºF |
Maximum Temperature |
N/A 420 ºF |
Compression Set @ 70 ºF |
N/A 16 % |
Compression Set @ 150 ºF |
N/A 24 % |
Compression Set @ 250 ºF |
N/A 31 % |
Compression Set @ 400 ºF |
N/A 35 % |
Color |
N/A Clear |
Chemical Resistance
Chemical Resistance |
N/A Kynar® resins demonstrate excellent resistance to an extensive array of chemicals. They resist attack from most inorganic acids and alkalis, aliphatic and aromatic hydrocarbons, organic acids, alcohols and halogenated solvents. However, strong alkalis (i.e. pH >12) and strong polar solvents such as acetone, ethyl acetate, dimethylformamide and dimethylacetamide can impede the effectiveness of Kynar® resins. |
Note
Note |
N/A
For information on your application, please contact the exclusive fabricator of KYNAR ULTRAFLEX™ elastomers: The statements, technical information and recommendations contained herein are believed to be accurate as of the time of printing. No warrantee of fitness for any purpose, or any other warrantee either expressed or implied, is made concerning the materials described herein. The user must thoroughly test the product prior to commercialization. No information provided can be used to develop patents, and the user is advised to take the appropriate steps to assure that this product will not result in patent infringement. |